Influence of the alloying elements on pitting corrosion of stainless steels: A modeling approach

B. Malki*, T. Souier, B. Baroux

*Corresponding author for this work

Research output: Contribution to journalArticlepeer-review

19 Citations (Scopus)

Fingerprint

Dive into the research topics of 'Influence of the alloying elements on pitting corrosion of stainless steels: A modeling approach'. Together they form a unique fingerprint.

Material Science