Estimating optimum compaction level for dense-graded Hot-Mix asphalt mixtures

Khalid Al Shamsi, Louay N. Mohammad

Research output: Contribution to journalArticle

2 Citations (Scopus)

Abstract

A critical step in the design of asphalt mixtures is laboratory compaction. Laboratory compaction should reflect field compaction and should produce mixtures that are economical and possess high structural stability. During the compaction process, asphalt mixtures are subjected to certain amount of compaction energy in order to achieve the required density. The Superpave volumetric mix design is based on compacting HMA mixtures to a specified compaction level described by the number of gyrations from the Superpave gyratory compactor (SGC). This level is termed Ndes and represents the required energy (based on the traffic level expected) to densify the mixture to a 4% air voids level. This paper re-examines the Superpave compaction requirements through extensive laboratory investigation of the response of a number of asphalt mixtures to the applied compaction energy. It also presents an alternative method to estimate the number of gyrations at which a mixture first reaches an optimum aggregate interlock and hence prevents overcompaction problems that might result in unstable aggregate structures or dry asphalt mixtures. A total of 12 HMA mixtures were studied. During compaction, force measurement was made using the pressure distribution analyzer (PDA). The compaction characteristics of the mixtures were analyzed using data from the PDA and the traditional Superpave Gyratory Compactor (SGC) results.

Original languageEnglish
Pages (from-to)11-21
Number of pages11
JournalJournal of Engineering Research
Volume7
Issue number1
Publication statusPublished - 2010

Fingerprint

Asphalt mixtures
Compaction
Superpave
Pressure distribution
Force measurement

Keywords

  • Asphalt mixtures
  • Laboratory compaction
  • Locking point
  • Mix design
  • Pavement materials

ASJC Scopus subject areas

  • Engineering(all)

Cite this

Estimating optimum compaction level for dense-graded Hot-Mix asphalt mixtures. / Al Shamsi, Khalid; Mohammad, Louay N.

In: Journal of Engineering Research, Vol. 7, No. 1, 2010, p. 11-21.

Research output: Contribution to journalArticle

@article{48cedc3364d74dca94a1d3daf71a047b,
title = "Estimating optimum compaction level for dense-graded Hot-Mix asphalt mixtures",
abstract = "A critical step in the design of asphalt mixtures is laboratory compaction. Laboratory compaction should reflect field compaction and should produce mixtures that are economical and possess high structural stability. During the compaction process, asphalt mixtures are subjected to certain amount of compaction energy in order to achieve the required density. The Superpave volumetric mix design is based on compacting HMA mixtures to a specified compaction level described by the number of gyrations from the Superpave gyratory compactor (SGC). This level is termed Ndes and represents the required energy (based on the traffic level expected) to densify the mixture to a 4{\%} air voids level. This paper re-examines the Superpave compaction requirements through extensive laboratory investigation of the response of a number of asphalt mixtures to the applied compaction energy. It also presents an alternative method to estimate the number of gyrations at which a mixture first reaches an optimum aggregate interlock and hence prevents overcompaction problems that might result in unstable aggregate structures or dry asphalt mixtures. A total of 12 HMA mixtures were studied. During compaction, force measurement was made using the pressure distribution analyzer (PDA). The compaction characteristics of the mixtures were analyzed using data from the PDA and the traditional Superpave Gyratory Compactor (SGC) results.",
keywords = "Asphalt mixtures, Laboratory compaction, Locking point, Mix design, Pavement materials",
author = "{Al Shamsi}, Khalid and Mohammad, {Louay N.}",
year = "2010",
language = "English",
volume = "7",
pages = "11--21",
journal = "Journal of Engineering Research",
issn = "1726-6009",
publisher = "Sultan Qaboos University",
number = "1",

}

TY - JOUR

T1 - Estimating optimum compaction level for dense-graded Hot-Mix asphalt mixtures

AU - Al Shamsi, Khalid

AU - Mohammad, Louay N.

PY - 2010

Y1 - 2010

N2 - A critical step in the design of asphalt mixtures is laboratory compaction. Laboratory compaction should reflect field compaction and should produce mixtures that are economical and possess high structural stability. During the compaction process, asphalt mixtures are subjected to certain amount of compaction energy in order to achieve the required density. The Superpave volumetric mix design is based on compacting HMA mixtures to a specified compaction level described by the number of gyrations from the Superpave gyratory compactor (SGC). This level is termed Ndes and represents the required energy (based on the traffic level expected) to densify the mixture to a 4% air voids level. This paper re-examines the Superpave compaction requirements through extensive laboratory investigation of the response of a number of asphalt mixtures to the applied compaction energy. It also presents an alternative method to estimate the number of gyrations at which a mixture first reaches an optimum aggregate interlock and hence prevents overcompaction problems that might result in unstable aggregate structures or dry asphalt mixtures. A total of 12 HMA mixtures were studied. During compaction, force measurement was made using the pressure distribution analyzer (PDA). The compaction characteristics of the mixtures were analyzed using data from the PDA and the traditional Superpave Gyratory Compactor (SGC) results.

AB - A critical step in the design of asphalt mixtures is laboratory compaction. Laboratory compaction should reflect field compaction and should produce mixtures that are economical and possess high structural stability. During the compaction process, asphalt mixtures are subjected to certain amount of compaction energy in order to achieve the required density. The Superpave volumetric mix design is based on compacting HMA mixtures to a specified compaction level described by the number of gyrations from the Superpave gyratory compactor (SGC). This level is termed Ndes and represents the required energy (based on the traffic level expected) to densify the mixture to a 4% air voids level. This paper re-examines the Superpave compaction requirements through extensive laboratory investigation of the response of a number of asphalt mixtures to the applied compaction energy. It also presents an alternative method to estimate the number of gyrations at which a mixture first reaches an optimum aggregate interlock and hence prevents overcompaction problems that might result in unstable aggregate structures or dry asphalt mixtures. A total of 12 HMA mixtures were studied. During compaction, force measurement was made using the pressure distribution analyzer (PDA). The compaction characteristics of the mixtures were analyzed using data from the PDA and the traditional Superpave Gyratory Compactor (SGC) results.

KW - Asphalt mixtures

KW - Laboratory compaction

KW - Locking point

KW - Mix design

KW - Pavement materials

UR - http://www.scopus.com/inward/record.url?scp=77958110520&partnerID=8YFLogxK

UR - http://www.scopus.com/inward/citedby.url?scp=77958110520&partnerID=8YFLogxK

M3 - Article

VL - 7

SP - 11

EP - 21

JO - Journal of Engineering Research

JF - Journal of Engineering Research

SN - 1726-6009

IS - 1

ER -